Tensile strength: 70MPa (yield)
Elongation: 15% (yield), 15% (fracture)
Impact strength: 108kJ/m2 (without notch), 7.6 kJ/m2 (with notch)
The synthesis of homo formaldehyde is generally condensation polymerization of formaldehyde aqueous solution in the presence of acid. A polyoxymethylene with a polymerization degree of more than 100 is obtained, which is then heated and decomposed into formaldehyde gas. After refining and dehydration, the monomer is usually purified by partial prepolymerization, and then polymerized in a dry solvent containing a small amount of initiator. Because of the presence of water, the molecular weight is significantly reduced. The initiator can be Lewis acid or alkali. However, most of them use tertiary amine for anionic addition polymerization. The reaction is as follows: the end group of polyoxymethylene is semi acetal (- CH2OH). When the temperature is higher than 100 ℃, the end group is easy to break, and generally needs to be stabilized by end group treatment. The heat resistance can reach 230 ℃ after stabilization treatment. Polyoxymethylene can be processed at 170~200 ℃, such as injection, extrusion, blow molding, etc. It is mainly used for engineering plastics, automobiles, mechanical parts, etc.
Dec 25, 2022
Leave a message
Performance Value Of POM
Previous
Characteristics Of POMNext
Structure Of POMSend Inquiry